Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3WG13 BK00102 - PA6-GF63 - BASF

Material Data Center offers the following functions for Ultramid® B3WG13 BK00102:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
Ultramid® B3WG13 BK00102 is a 63% glass filled, injection molding, high modulus Polyamid designed to have high strength and stiffness for metal replacement applications. It also has excellent moldability and outstanding surface appearance.

Applications:
Potential applications are mirror brackets, fuel lids, gas-assisted steering wheel inserts, ski bindings and bike rack clamps.
Механические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 22400 / - МПа ISO 527
Напряжение при разрыве 235 / - МПа ISO 527
Удлинение при разрыве 2 / - % ISO 527
Ударная вязкость по Шарпи, +23°C 90 / - кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи, -30°C 90 / - кДж/м2 ISO 179/1eU
Ударная вязкость по Шарпи с надрезом, +23°C 15 / - кДж/м2 ISO 179/1eA
Ударная вязкость по Шарпи с надрезом, -30°C 13 / - кДж/м2 ISO 179/1eA
Теплофизические свойствасухой / кондЕдиницаСтандарт
Данные ISO
Температура плавления, 10°C/мин 220 / * °C ISO 11357-1/-3
Температура изгиба под нагрузкой, 1.80 МПа 214 / * °C ISO 75-1/-2
Класс горючести при номинальной толщине 1.5 мм HB / * класс IEC 60695-11-10
Толщина образца 1.5 / * мм -
желтая карточка (Yellow Card) да / * - -
Класс горючести при толщине образца h HB / * класс IEC 60695-11-10
Толщина образца 3.0 / * мм -
желтая карточка (Yellow Card) да / * - -
Прочие свойствасухой / кондЕдиницаСтандарт
Плотность 1740 / - кг/м³ ISO 1183
Рекомендации по переработке литьем под давлениемЗначениеЕдиницаСтандарт
Температура предварительной сушки 80 °C -
Влажность переработки ≤0.03 % -
Температура расплава 300 - 320 °C -
Температура формы 80 - 95 °C -
Диаграммы
Вязкость - скорость сдвига , Ultramid® B3WG13 BK00102, PA6-GF63, BASF
Касательное напряжение - скорость сдвига , Ultramid® B3WG13 BK00102, PA6-GF63, BASF
Напряжение - удлинение , Ultramid® B3WG13 BK00102 (сухой), PA6-GF63, BASF
Напряжение - удлинение , Ultramid® B3WG13 BK00102 (усл.), PA6-GF63, BASF
Секущая модуля упругости - удлинение , Ultramid® B3WG13 BK00102 (сухой), PA6-GF63, BASF
Секущая модуля упругости - удлинение , Ultramid® B3WG13 BK00102 (усл.), PA6-GF63, BASF
Особые свойства и характеристики
Способы переработки
Литье под давлением
Вид поставки
Гранулы, Черный
Особые показатели
Термостабилизированный или стойкий к воздействию тепла
Доступность материала по регионам
Северная Америка
Другая текстовая информация
Литье под давлением
PREPROCESSING
Max. Water content: 0.03%
Although Product is supplied in sealed containers, drying is recommended in applications requiring optimum surface aesthetics. A dehumidifying or desiccant dryer operating at 80 °C (176 °F) is recommended. Drying time is dependent on moisture level.
Further information concerning safe handling procedures can be obtained from the Material Safety Data Sheet. Alternatively, please contact your BASF representative.

PROCESSING
Melt Temperature 300-320 °C (572-608 °F)
Mold Temperature 80-95 °C (176-203 °F)
Injection and Packing Pressure 35-125 bar (500-1500psi)
Rear Zone 275-300 °C (527-572 °F)
Center Zone 285-310 °C (545-590 °F)
Front Zone 300-325 °C (572-617 °F)
Nozzle 300-325 °C (572-617 °F)

This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics arecritical, a mold surface temperature of 80-95 °C (176-203 °F) is required.

Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.

Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage.

Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.